产品说明Product description | ||||||||
·ES10D-11是一款高回弹性透明材料,具有极好的耐刮擦性和耐候性。 ·ES10D-11 is a kind of high resilience and translucent material which has excellent scratch resistance and weather resistance properties. | ||||||||
关键特性Key characteristic | ||||||||
1. 耐老化性优良,不易黄变excellent ageing resistance and not easy to yellowing 2. 表面哑,手感柔软干爽。dumb surface,soft and dry touch 3. 模量高,不易变形high modulus,not easy to deformation 4. 成型快,不粘模具rapid molding,non-stick mold | ||||||||
功能Function | ||||||||
产品应用 Main application | 玩具产品Toy products | 挤出管 Extruded tube | ||||||
运动器材Sports equipment | ||||||||
加工方法Processing method | 注塑成型Injection molding 挤出成型Extrusion molding | |||||||
环保认证 Environmental certification | ROHS | REACH | EN71-3 | |||||
PAHS | ASTM-F963 | Phthalate | ||||||
颜色Color | 透明Translucent | |||||||
气味Smell | 少许树脂味A little resin smell | |||||||
外型Appearance | 圆球形小颗粒Cylindrical particle,about 3mm×1.5mm | |||||||
储藏期Storage period | 常温下通风干燥,24个月Ventilated dry at normal temperature,about 24 months | |||||||
包装方式Packaging method | 25公斤/袋 25kg/bag | |||||||
物理性能Physical properties | 结果Result | 单位Unit | 方法Method | 成型条件Molding condition | ||||
比重Specific gravity | 0.89±0.02 | g/cm3 | ASTM D792 | 干燥温度Drying temp 60℃ | ||||
硬度Hardness | 10±5 | shoreA | ASTM D2240 | 干燥时间Drying time 2Hours | ||||
拉伸强度Tensile strength | >2 | Mpa | ASTM D412 | 射嘴温度Nozzle temp 200℃ | ||||
断裂延伸Elongation at break | >500 | % | ASTM D412 | 螺筒一段温度Screw 1 temp 190℃ | ||||
撕裂强度Tearing strength | >7 | Kn/m | ASTM D624 | 螺筒二段温度Screw 2 temp 180℃ | ||||
熔融指数Melt index | >3 | g/10min | ASTM D1238 | 螺筒三段温度Screw 3 temp 170℃ | ||||
注意事项Matters need attention | ||||||||
清洗料管 Purge compound | 需使用PP或 PE清洗干净机台螺杆,且把机台射嘴彻底清除干净please make sure you that you have cleaned the machine screw with PP or PE, and put the machine nozzle thoroughly clean | |||||||
着色 Coloring
| 请选择以PE或EVA为基材之色母,切勿使用以PVC为基材者。另外加工时请采用较高的螺杆转速和较高的背压,才能让着色剂达到较好的分散效果Please select color master batch on PE or EVA material with the exception of PVC.Higher screw speed and backpressure and needed for better colorant dispersion | |||||||
回收 Recycling | 二次料(水口料)回收比率建议最多20%。 Consistent regrind usage of up to 20% is permissible |