倍韧/BESTPERNE®ES45D-11
热塑性弹性体Thermoplastic Elastomer
产品说明Product description | |||||||
·ES45D-11是一款高回弹性透明材料,具有极好的耐刮擦性和耐候性。 ·ES45D-11 is a kind of high resilience and translucent material which has excellent scratch resistance and weather resistance properties.
| |||||||
关键特性Key characteristic | |||||||
1. 耐老化性优良,不易黄变excellent ageing resistance and not easy to yellowing 2. 表面哑,手感柔软干爽。dumb surface,soft and dry touch 3. 模量高,不易变形high modulus,not easy to deformation 4. 成型快,不粘模具rapid molding,non-stick mold | |||||||
功能Function | |||||||
产品应用 Main application | 玩具产品Toy products | 挤出管 Extruded tube | |||||
运动器材Sports equipment | 脚轮Truckles | ||||||
加工方法Processing method | 注塑成型Injection molding 挤出成型Extrusion molding | ||||||
环保认证 Environmental certification | ROHS | REACH | EN71-3 | ||||
PAHS | ASTM-F963 | Phthalate | |||||
颜色Color | 透明Translucent | ||||||
气味Smell | 少许树脂味A little resin smell | ||||||
外型Appearance | 圆球形小颗粒Cylindrical particle,about 3mm×1.5mm | ||||||
储藏期Storage period | 常温下通风干燥,24个月Ventilated dry at normal temperature,about 24 months | ||||||
包装方式Packaging method | 25公斤/袋 25kg/bag | ||||||
物理性能Physical properties | 结果Result | 单位Unit | 方法Method | 成型条件Molding condition | |||
比重Specific gravity | 0.89±0.02 | g/cm3 | ASTM D792 | 干燥温度Drying temp 70℃ | |||
硬度Hardness | 45±5 | shoreA | ASTM D2240 | 干燥时间Drying time 2Hours | |||
拉伸强度Tensile strength | >4 | Mpa | ASTM D412 | 射嘴温度Nozzle temp 210℃ | |||
断裂延伸Elongation at break | >450 | % | ASTM D412 | 螺筒一段温度Screw 1 temp 200℃ | |||
撕裂强度Tearing strength | >18 | Kn/m | ASTM D624 | 螺筒二段温度Screw 2 temp 190℃ | |||
熔融指数Melt index | <9 | g/10min | ASTM D1238 | 螺筒三段温度Screw 3 temp 160℃ |