倍韧/BESTPERNE® 3818H-3
熱塑性彈性體Thermoplastic Elastomer
產品說明Product description | |||||||
·3818H-3是一款高性能材料,耐黄变非常出色,具有非常强劲的包胶粘接强度和特别舒适的手感。可快速成型。. 3818H-3 is a high performance material, the yellow stain is very good, has a very strong adhesive bond strength and special comfortable feel. Rapid prototyping. . | |||||||
關鍵特性Key characteristic | |||||||
1.表面哑,手感细腻柔软。Smooth surface, feel fine and soft 2.粘接强度非常高,可粘接材质:ABS.PC。Bond strength is very high, can be bonded material: ABS.PC. 3.成型快、不粘模具。Forming fast, non stick mold 4.表面耐刮擦,不易起毛屑。The surface scratch resistant, not easy pilling chip | |||||||
功能Function | |||||||
产品应用 main application | 仪器外壳Instrument case | 医疗器材Medical equipment | |||||
高档手机护套High quality mobile phone sheath | 电子器件粘胶配件Electronic plastic accessories | ||||||
加工方法Processing method | 注塑成型Injection molding | ||||||
环保认证 Environmental certification | ROHS | REACH | EN71-3 | ||||
PAHS | ASTM-F963 | Phthalate | |||||
颜色Color | 本色 | ||||||
气味Smell | 少许树脂味A little resin smell | ||||||
外型Appearance | 圆球形小颗粒Cylindrical particle,about 3mm×1.5mm | ||||||
储藏期Storage period | 常温下通风干燥,24个月Ventilated dry at normal temperature,about 24 months | ||||||
包装方式Packaging method | 25公斤/袋 25kg/bag | ||||||
物理性能Physical properties | 结果Result | 单位Unit | 方法Method | 成型条件Molding condition | |||
比重Specific gravity | 1.16±0.02 | g/cm3 | ASTM D792 | 干燥温度Drying temp 90℃ | |||
硬度Hardness | 93±3 | shoreA | ASTM D2240 | 干燥时间Drying time 3Hours | |||
拉伸强度Tensile strength | >12 | Mpa | ASTM D412 | 射嘴温度Nozzle temp 200℃ | |||
断裂延伸Elongation at break | >400 | % | ASTM D412 | 螺筒一段温度Screw 1 temp 200℃ | |||
撕裂强度Tearing strength | >75 | Kn/m | ASTM D624 | 螺筒二段温度Screw 2 temp 180℃ | |||
熔融指数Melt index | >10 | g/10min | ASTM D1238 | 螺筒三段温度Screw 3 temp 180℃ |