倍韧/BESTPERNE® EN65A-11
热塑性弹性体Thermoplastic Elastomer
产品说明Product description | ||||
EN65A-11是一款以SEBS为主基材的热塑性弹性体,成型快,好配色。 EN65A-11 is a kind of thermoplastic elastomer material based on SEBS as main material.Also it has rapid molding and easy coloring properties.
| ||||
关键特性Key characteristic | ||||
1.手感柔软细腻,干爽,耐刮擦性好。Exquisite, soft and dry touch,good scratch resistance. 2.抗老化及耐腐蚀性优良。Excellent ageing resistance and corrosion resistance 3.可以包PP,PE It can be spliced with PP and PE | ||||
功能Function | ||||
产品应用 Main application | 1 汽车用品 Automotive products | 3手把Handlebar | ||
2 运动器材Sports equipment | 4玩具产品Toy products | |||
加工方法Processing method | 注塑成型Injection molding | |||
环保认证 Environmental certification | ROHS | REACH | EN71-3 | |
PAHS | ASTM-F963 | Phthalate | ||
颜色Color | 本色 Natural | |||
气味Smell | 少许树脂味A little resin smell | |||
外型Appearance | 圆球形小颗粒Cylindrical particle,about 3mm×1.5mm | |||
储藏期Storage period | 常温下通风干燥,24个月Ventilated dry at normal temperature,about 24 months | |||
包装方式Packaging method | 25公斤/袋 25kg/bag |