倍韧/BESTPERNE® EN95A1-01
热塑性弹性体Thermoplastic Elastomer
产品说明Product description | |||||||
·EN95A1-01是一款高性能的高分子材料,强度高,耐黄变好,耐化学性能优良。 ·EN95A1-01 is a kind of high performance polymer material which has high strength,excellent yellowing resistance and chemical solvent resistance properties. | |||||||
关键特性Key characteristic | |||||||
1.表面光亮,bright surface 2.弹性优良,易成型。excellent elasticity,easy forming 3.可粘接PP,PE,强度非常高very high bonding strength, adhesive material:PP、PE | |||||||
功能Function | |||||||
产品应用 Main application | 1 汽车用品Automotive products | 3电子产品Electronic products | |||||
2 运动器材Sports equipment | 4家具产品Furniture products | ||||||
加工方法Processing method | 注塑成型Injection molding | ||||||
环保认证 Environmental certification | ROHS | REACH | EN71-3 | ||||
PAHS | ASTM-F963 | Phthalate | |||||
颜色Color | 本色 Natural | ||||||
气味Smell | 少许树脂味A little resin smell | ||||||
外型Appearance | 圆球形小颗粒Cylindrical particle,about 3mm×1.5mm | ||||||
储藏期Storage period | 常温下通风干燥,24个月Ventilated dry at normal temperature,about 24 months | ||||||
包装方式Packaging method | 25公斤/袋 25kg/bag | ||||||
物理性能Physical properties | 结果Result | 单位Unit | 方法Method | 成型条件Molding condition | |||
比重Specific gravity | 0.98±0.02 | g/cm3 | ASTM D792 | 干燥温度Drying temp 80℃ | |||
硬度Hardness | 53±3 | shoreD | ASTM D2240 | 干燥时间Drying time 2Hours | |||
拉伸强度Tensile strength | >10 | Mpa | ASTM D412 | 射嘴温度Nozzle temp 190℃ | |||
断裂延伸Elongation at break | <450 | % | ASTM D412 | 螺筒一段温度Screw 1 temp 180℃ | |||
撕裂强度Tearing strength | >80 | Kn/m | ASTM D624 | 螺筒二段温度Screw 2 temp 170℃ | |||
熔融指数Melt index | >3 | g/10min | ASTM D1238 | 螺筒三段温度Screw 3 temp 160℃ |