倍韧/BESTPERNE® SP-16
热塑性弹性体Thermoplastic Elastomer
产品说明Product description | ||||||
·SP-16是一款无卤阻燃、新型高分子材料。 ·SP-16 is a new kind of polymer material which is halogen-free flame retardant.
| ||||||
关键特性Key characteristic | ||||||
1.表面哑,手感细腻柔软。Dumb surface, exquisite and soft touch 2.成型快、不粘模具。Rapid molding,non-stick mold 3.耐候性好。Excellent weather resistance. 4.阻燃等级:可达到UL94-V0。Flame retardant rating:UL94-V0
| ||||||
功能Function | ||||||
产品应用 Main application | 1电线、电缆护套Protecting coat of cables and wires | 3汽车挡泥板Car fenders | ||||
2密封垫Sealing gaskets | 4排挡罩Gear covers | |||||
加工方法Processing method | 注塑成型Injection molding | |||||
环保认证 Environmental certification | ROHS | REACH | EN71-3 | |||
PAHS | ASTM-F963 | Phthalate | ||||
颜色Color | 米黄Beige | |||||
气味Smell | 少许树脂味A little resin smell | |||||
外型Appearance | 圆球形小颗粒Cylindrical particle,about 3mm×1.5mm | |||||
储藏期Storage period | 常温下通风干燥,24个月Ventilated dry at normal temperature,about 24 months | |||||
包装方式Packaging method | 25公斤/袋 25kg/bag | |||||
物理性能Physical properties | 结果Result | 单位Unit | 方法Method | 成型条件Molding condition | ||
比 重Specific gravity | 1.14±0.02 | g/cm3 | ASTM D792 | 干燥温度Drying temp 90℃ | ||
硬 度Hardness | 72±5 | shoreA | ASTM D2240 | 干燥时间Drying time 2Hours | ||
拉伸强度Tensile strength | >6 | Mpa | ASTM D412 | 射嘴温度Nozzle temp 200℃ | ||
断裂延伸Elongation at break | >300 | % | ASTM D412 | 螺筒一段温度Screw 1 temp 190℃ | ||
撕裂强度Tearing strength | >25 | Kn/m | ASTM D624 | 螺筒二段温度Screw 2 temp 180℃ | ||
熔融指数Melt index | >1 | g/10min | ASTM D1238 | 螺筒三段温度Screw 3 temp 170℃ |