倍韧/BESTPERNE® TFU6066
热塑性弹性体Thermoplastic Elastomer
产品说明Product description | |||||||
TFU6066是一款新型的高分子复合材料,韧性和强度平衡,耐磨,抗污。丝滑细腻,超耐黄变,耐化学性,导热性符合穿戴产品的要求。 TFU6066is a new type of polymer composites, toughness and strength balance, wear and dirt. Silky smooth, ultra-yellowing resistance, chemical resistance, thermal conductivity, in line with the requirements of wearable products. | |||||||
关键特性Key characteristic | |||||||
1舒适的触感,柔韧细腻、爽滑。comfortable feel,flexible ,exquisite and smooth touch. 2粘接强度高,可粘接材质ABS .PC .TPU very high bonding strength, adhesive material:ABS, PC,TPU. 3实用性,耐脏、耐油、耐汗、耐菌、耐变色It is very practical,for excellent stain resistance,oil resistance,sweat resistance bacteria resistance and discoloration resistance. 4具有TPU的强度,耐磨和硅胶的柔韧细腻the strength of TPU,exquisite and flexible touch are similar to Silicone. 5绝对可靠的安全性,无毒、过敏性reliable security ,non-toxic,non-allergic. | |||||||
功能Function | |||||||
产品应用 Main application | 手腕带Bracelets | 高档手机护套High-end phone protective covers | |||||
医疗器材Medical device | 电子器件粘胶配件Electronic plastic accessories | ||||||
加工方法Processing method | 注塑成型Injection molding | ||||||
环保认证 Environmental certification | ROHS | REACH | EN71-3 | ||||
PAHS | ASTM-F963 | Phthalate | |||||
颜色Color | 本色 | ||||||
气味Smell | 少许树脂味A little resin smell | ||||||
外型Appearance | 圆球形小颗粒Cylindrical particle,about 3mm×1.5mm | ||||||
储藏期Storage period | 常温下通风干燥,24个月Ventilated dry at normal temperature,about 24 months | ||||||
包装方式Packaging method | 25公斤/袋 25kg/bag | ||||||
物理性能Physical properties | 结果Result | 单位Unit | 方法Method | 成型条件Molding condition | |||
比重Specific gravity | 1.13±0.02 | g/cm3 | ASTM D792 | 干燥温度Drying temp 90℃ | |||
硬度Hardness | 63±5 | shoreA | ASTM D2240 | 干燥时间Drying time 2Hours | |||
拉伸强度Tensile strength | >10 | Mpa | ASTM D412 | 射嘴温度Nozzle temp 180℃ | |||
断裂延伸Elongation at break | <800 | % | ASTM D412 | 螺筒一段温度Screw 1 temp 170℃ | |||
撕裂强度Tearing strength | >45 | Kn/m | ASTM D624 | 螺筒二段温度Screw 2 temp 160℃ | |||
熔融指数Melt index | >10 | g/10min | ASTM D1238 | 螺筒三段温度Screw 3 temp 150℃ |