倍韧/BESTPERNE® TN70N-TT
熱塑性彈性體Thermoplastic Elastomer
產品說明Product description | |||||||
·TN70N-TT是一款高性能高分子材料,与尼龙的粘接强度高。材料耐高温。不粘模具,可快速成型。 ·TN70N-TT is a high performance polymer material, and the high bonding strength of nylon. Material resistance to high temperature. Non stick mold, can be rapid prototyping. | |||||||
關鍵特性Key characteristic | |||||||
1. 表面哑,手感细腻柔软。dumb surface, exquisite and soft feeling 2. 粘接强度非常高,可粘接材质: PA. 3. 成型快、不粘模具。rapid molding,non-stick mold 4. 表面耐刮擦,不易起毛屑。scratch resistance on the surface,not easy to fluff | |||||||
功能Function | |||||||
产品应用 main application | 工具手把Tool hand | 汽车产品Automotive products | |||||
仪器外壳Instrument housing | |||||||
加工方法Processing method | 注塑成型Injection molding | ||||||
环保认证 Environmental certification | ROHS | REACH | EN71-3 | ||||
PAHS | ASTM-F963 | Phthalate | |||||
颜色Color | 本色 | ||||||
气味Smell | 少许树脂味A little resin smell | ||||||
外型Appearance | 圆球形小颗粒Cylindrical particle,about 3mm×1.5mm | ||||||
储藏期Storage period | 常温下通风干燥,24个月Ventilated dry at normal temperature,about 24 months | ||||||
包装方式Packaging method | 25公斤/袋 25kg/bag | ||||||
物理性能Physical properties | 结果Result | 单位Unit | 方法Method | 成型条件Molding condition | |||
比重Specific gravity | 1.15±0.02 | g/cm3 | ASTM D792 | 干燥温度Drying temp 90℃ | |||
硬度Hardness | 70±5 | shoreA | ASTM D2240 | 干燥时间Drying time 3Hours | |||
拉伸强度Tensile strength | >6 | Mpa | ASTM D412 | 射嘴温度Nozzle temp 230℃ | |||
断裂延伸Elongation at break | >400 | % | ASTM D412 | 螺筒一段温度Screw 1 temp 220℃ | |||
撕裂强度Tearing strength | >42 | Kn/m | ASTM D624 | 螺筒二段温度Screw 2 temp 210℃ | |||
熔融指数Melt index | >2 | g/10min | ASTM D1238 | 螺筒三段温度Screw 3 temp 200℃ |