倍韧/BESTPERNE® TU8008
热塑性弹性体Thermoplastic Elastomer
产品说明Product description | ||||||||
·TU8008是一款聚醚类聚氨酯材料.可以快速成型性,不粘模具。高强度,高回复性。 ·TU8008is a polyether polyurethane material. It can be rapid prototyping, non stick mold. High strength, high recovery.
| ||||||||
关键特性Key characteristic | ||||||||
1.高强度,高韧性High strength and high toughness. 2.超高的耐磨性和回弹性Excellent wear resistance and high resilience. 3.成型速度快,不析出Rapid molding,no precipitation. 4.可通过4级耐黄变。Can pass the four level resistance to yellowing | ||||||||
功能Function | ||||||||
产品应用 Main application | 手机保护套Phone protective cover | 电脑产品Computer products | ||||||
仪器外壳Instrument shell | 体育用品Sports equipment | |||||||
加工方法Processing method | 注塑成型Injection molding 挤出成型 Extrusion molding | |||||||
环保认证 Environmental certification | ROHS | REACH | EN71-3 | |||||
PAHS | ASTM-F963 | Phthalate | ||||||
颜色Color | 透明Transparent | |||||||
气味Smell | 少许树脂味A little resin smell | |||||||
外型Appearance | 圆球形小颗粒Cylindrical particle,about 3mm×1.5mm | |||||||
储藏期Storage period | 常温下通风干燥,12个月Ventilated dry at normal temperature,about 12 months | |||||||
包装方式Packaging method | 25公斤/袋 25kg/bag | |||||||
物理性能Physical properties | 结果Result | 单位Unit | 方法Method | 成型条件Molding condition | ||||
比重Specific gravity | 1.15±0.02 | g/cm3 | ASTM D792 | 干燥温度Drying temp 90℃ | ||||
硬度Hardness | 80±5 | shoreA | ASTM D2240 | 干燥时间Drying time 3Hours | ||||
拉伸强度Tensile strength | >15 | Mpa | ASTM D412 | 射嘴温度Nozzle temp 200℃ | ||||
断裂延伸Elongation at break | <900 | % | ASTM D412 | 螺筒一段温度Screw 1 temp 190℃ | ||||
撕裂强度Tearing strength | >60 | Kn/m | ASTM D624 | 螺筒二段温度Screw 2 temp 180℃ | ||||
熔融指数Melt index | >4 | g/10min | ASTM D1238 | 螺筒三段温度Screw 3 temp 170℃ | ||||
注意事项Matters need attention | ||||||||
清洗料管 Purge compound | 需使用PP或 PE清洗干净机台螺杆,且把机台射嘴彻底清除干净Please make sure you that you have cleaned the machine screw with PP or PE, and put the machine nozzle thoroughly clean. | |||||||
着色 Coloring
| 请选择以PE或EVA为基材之色母,切勿使用以PVC为基材者。另外加工时请采用较高的螺杆转速和较高的背压,才能让着色剂达到较好的分散效果Please select color master batch on PE or EVA material with the exception of PVC.Higher screw speed and backpressure are needed for better colorant dispersion. | |||||||
回收 Recycling | 二次料(水口料)回收比率建议最多5%. Consistent regrind usage of up to 5% is permissible. |