产品分类: PP熔喷料
    订购热线:13829234372/13922538943

      技术资料表

      Technical Data Sheet(TDS)

      产品信息 Product information

      品牌

      Brand

      易来极

      ELE KEY

      材料类型

      Material Type

      PP油性母粒

      PP Oiliness Masterbatch

      牌号

      Geade

      S0511

      特性 Characteristic

      ·亲油配方,提高油性颗粒物Lipophilic formula to improve oily particles


      ·分散性能极佳Excellent dispersion


      ·稳定出丝Stable filament


      ·增大调机工艺参数窗口Increase the window of adjusting process parameters

      外观 Appearance

      ·圆柱状 3.5-8mm    Cylindrical shape

      颜色 Colour

      ·本白色            Natural

      气味 Smell

      ·接近无味          Almost tasteless

      包装Packing

      ·25KG/包           KG/ package

      用途Applications

      ·熔喷无纺布        Melt Blown Monwoven


      ·与绝大多数的熔喷聚丙烯相熔性良好,直接添加,提高油性颗粒物过滤量,改善发硬变脆现象It has good fusibility with the majority of melt blown polypropylene and can be directly added to improve the filtration amount of oily particles and improve the hardening and embrittlement

      通用性能 General Properties

      序号

      No.

      性能

      Properties

      测试值

      Value

      单位

      Unit

      检验方法

      Method

      测试条件

      Test conditon

      1

      熔体流动速率Melt Flow Index

      200±100

      g/10min

      GB/T 3682

      230℃,2.16kg

      2

      熔点Melting Point

      160

      ℃

      GB/T 19466

      10℃/min

      3

      含水量Water content

      < 0.03

      %

      GB/T 6283-2008

      23℃  75%

      4

      密度density

      0.90

      g/cm3

      GB/T 4472-2011

      23℃  75%

      5

      建议添加量Recommended addition   10-20%

       

       

      备注

      Remarks

       

      塑伯S0511油性颗粒物过滤量提升母粒是针对大部分客户对于油性颗粒物过滤量要求(FFP2标准)推出的新产品。采用亲油性的配方工艺,均匀分散于PP(聚丙烯)载体中,成丝后对油性颗粒物具有同性相吸效应,对过滤量的提升与添加量成正比例(建议添加20%以下),随着添加比例增加,熔体流动性降低,故成型温度应同步提高。

      SPP S0511 oil particle filter quantity promotion masterbatch is a new product launched for most customers' requirements for oil particle filter quantity (FFP2 standard).The formulation process with lipophilic property is adopted, which is evenly dispersed in PP (polypropylene) carrier. After being spun, it has the same phase absorption effect on oily particles. The increase of filtration amount is in positive proportion to the addition amount (it is suggested to add less than 20%). With the increase of the addition proportion, the melt fluidity decreases, so the molding temperature should be increased synchronously.

       

      以上数据为我公司测量之理论数据仅供参考,版权所有@广东塑伯新材料有限公司

      The above data for the theory of the measurement data of our company, for your reference only. Copyright @ SPP New 



      如需了解更多产品信息,请联系我们:

      销售专员:

      廖流爱:13922538943(微信/手机同号)

      李小姐:13826903196(微信/手机同号)

      李明霞:13829234372(微信/手机同号)

      技术支持:

      廖慈华:13602342196(微信/手机同号)




      0
      * 表示必填采购:PP油性母粒S0511 油性测试专用母粒
      * 联系人: 请填写您的真实姓名
      公司名称: 请填写您的公司名称
      联系电话:
      * 手机号码: 请填写您的联系电话
      *QQ:
      联系地址:
      * 采购意向描述:
      请填写采购的产品数量和产品描述,方便我们进行统一备货。
      验证码: 验证码
      我要评论:  
      内 容:
      (内容最多500个汉字,1000个字符)
      验证码: 看不清?!