桶装水盖专用材料,普通级通用
50T-15是一款经济型半透明材料,具有优异的耐刮擦效果。
50T-15 is a kind of economical and translucent material which has excellent scratch resistance property.
50T-15是一款经济型半透明材料,具有优异的耐刮擦效果。
50T-15 is a kind of economical and translucent material which has excellent scratch resistance property.
关键特性Key characteristic
1.表面哑,手感细腻柔软Dumb surface, exquisite and soft touch.
2.粘接强度非常高,可粘接材质:PP,PE. Very high bonding strength,adhesive materials:PP and PE.
3.成型快、不粘模具Rapid molding and non-stick mold.
4.表面耐刮擦,不易起毛屑Scratch resistance on the surface,not easy to fluff.
1.表面哑,手感细腻柔软Dumb surface, exquisite and soft touch.
2.粘接强度非常高,可粘接材质:PP,PE. Very high bonding strength,adhesive materials:PP and PE.
3.成型快、不粘模具Rapid molding and non-stick mold.
4.表面耐刮擦,不易起毛屑Scratch resistance on the surface,not easy to fluff.
产品应用 饭盒盖包胶Rubber coating of lunch-box cover
Main application 玩具产品Toy products
加工方法Processing method 注塑成型Injection molding
环保认证 FDA ROHS REACH EN71-3 PAHS ASTM-F963 Phthalate
Environmental certification
颜色Color: 半透明 Translucent
气味Smell : 少许树脂味A little resin smell
外型Appearance: 圆球形小颗粒Cylindrical particle,about 3mm×1.5mm
储藏期Storage period: 常温下通风干燥,24个月Ventilated dry at normal temperature,about 24 months
包装方式Packaging method: 25公斤/袋 25kg/bag
Environmental certification
颜色Color: 半透明 Translucent
气味Smell : 少许树脂味A little resin smell
外型Appearance: 圆球形小颗粒Cylindrical particle,about 3mm×1.5mm
储藏期Storage period: 常温下通风干燥,24个月Ventilated dry at normal temperature,about 24 months
包装方式Packaging method: 25公斤/袋 25kg/bag
物理性能Physical properties
比重Specific gravity 0.92±0.02g/cm3
硬度Hardness 47±5shoreA
拉伸强度Tensile strength >3Mpa
断裂延伸Elongation at break <650%
撕裂强度Tearing strength >14Kn/m
熔融指数Melt index >3g/10min
比重Specific gravity 0.92±0.02g/cm3
硬度Hardness 47±5shoreA
拉伸强度Tensile strength >3Mpa
断裂延伸Elongation at break <650%
撕裂强度Tearing strength >14Kn/m
熔融指数Melt index >3g/10min
注意事项Matters need attention:
清洗料管 Purge compound:
需使用PP或 PE清洗干净机台螺杆,且把机台射嘴彻底清除干净.
Please make sure you that you have cleaned the machine screw with PP or PE, and put the machine nozzle thoroughly clean.
清洗料管 Purge compound:
需使用PP或 PE清洗干净机台螺杆,且把机台射嘴彻底清除干净.
Please make sure you that you have cleaned the machine screw with PP or PE, and put the machine nozzle thoroughly clean.
着色Coloring:
请选择以PE或EVA为基材之色母,切勿使用以PVC为基材者。另外加工时请采用较高的螺杆转速和较高的背压,才能让着色剂达到较好的分散效果Please select color master batch on PE or EVA material with the exception of PVC.Higher screw speed and backpressure are needed for better colorant dispersion.
请选择以PE或EVA为基材之色母,切勿使用以PVC为基材者。另外加工时请采用较高的螺杆转速和较高的背压,才能让着色剂达到较好的分散效果Please select color master batch on PE or EVA material with the exception of PVC.Higher screw speed and backpressure are needed for better colorant dispersion.
如需了解更多产品信息,请联系我们:
销售专员:
廖流爱:13922538943(微信/手机同号)
李小姐:13826903196(微信/手机同号)
李明霞:13829234372(微信/手机同号)
技术支持:
廖慈华:13602342196(微信/手机同号)
* 表示必填采购:50T-15
| * 联系人: | 请填写您的真实姓名 |
| * 手机号码: | 请填写您的联系电话 |
| *QQ: | |
| * 采购意向描述: | |
| 请填写采购的产品数量和产品描述,方便我们进行统一备货。 | |
| 验证码: |
|
相关资讯
| 我要评论: | |
| 内 容: |
(内容最多500个汉字,1000个字符) |
| 验证码: | 看不清?! |










共有-条评论【我要评论】