收藏本站|常见问答|联系塑伯|网站地图

您好!欢迎访问塑伯公司TPE,TPR官方网站!
TPE,TPR,广东塑伯新材料有限公司

塑伯官方微博 :塑伯官方微博

咨询热线13829234372/13922538943

倍韧TPE

85S

产品分类: 倍韧TPE
    订购热线:13829234372/13922538943

      倍韧/BESTPERNE®  85S

      热塑性弹性体Thermoplastic Elastomer

      产品说明Product description

      ·85S是一款高透明材料,具有良好的抗冲击和抗疲劳性能。

      ·85S is a kind of high transparent material which has excellent impact resistance and fatigue resistance properties.

      关键特性Key characteristic

      1.粘接强度非常好,可粘接材质:PS,ABS,PC  Very high bonding strength,adhesive materials:PS,ABS and PC.

      2.表面光亮Bright surface.

      3.可噴油,絲印,上膠水,油墨Oil injection,silkscreen,can be applied with glue and ink.

      4.良好的耐磨性,耐抗拉,耐撕裂性能Excellent abrasion resistance,tension resistance and tear resistance.

      功能Function

      产品应用

      Main application

      玩具公仔Toy dolls

      泳鏡粘PC Swimming glasses PC

      电动牙刷Electric toothbrush


      加工方法Processing method

      注塑成型Injection molding

      环保认证

      Environmental certification

      ROHS

      REACH

      EN71-3

      PAHS

      ASTM-F963

      Phthalate

      颜色Color

      透明Transparent

      气味Smell

      少许树脂味A little resin smell

      外型Appearance

      圆球形小颗粒Cylindrical particle,about 3mm×1.5mm

      储藏期Storage period

      常温下通风干燥,24个月Ventilated dry at normal temperature,about 24 months

      包装方式Packaging method

      25公斤/袋 25kg/bag

      物理性能Physical properties

      结果Result

      单位Unit

      方法Method

      成型条件Molding condition

      比重Specific gravity

      0.94±0.02

      g/cm3

      ASTM D792

      干燥温度Drying temp     50 ℃

      硬度Hardness

      83±5

      shoreA

      ASTM D2240

      干燥时间Drying time      2h

      拉伸强度Tensile strength

      >6

      Mpa

      ASTM D412

      射嘴温度Nozzle temp     190℃

      断裂延伸Elongation at break

      >350

      %

      ASTM D412

      螺筒一段温度Screw 1 temp 180℃

      撕裂强度Tearing strength

      >30

      Kn/m

      ASTM D624

      螺筒二段温度Screw 2 temp 170℃

      熔融指数Melt index

      >10

      g/10min

      ASTM D1238

      螺筒三段温度Screw 3 temp 160℃

      注意事项Matters need attention

      清洗料管

      Purge compound

      需使用PP或 PE清洗干净机台螺杆,且把机台射嘴彻底清除干净Please make sure you that you have cleaned the machine screw with PP or PE, and put the machine nozzle thoroughly clean.

      着色

      Coloring

       

       

      请选择以PE或EVA为基材之色母,切勿使用以PVC为基材者。另外加工时请采用较高的螺杆转速和较高的背压,才能让着色剂达到较好的分散效果Please select color master batch on PE or EVA material with the exception of PVC.Higher screw speed and backpressure are needed for better colorant dispersion.

      回收

      Recycling

      二次料(水口料)回收比率建议最多5%.

      Consistent regrind usage of up to 5% is permissible.

      以上数据为我公司测量之理论数据仅供参考,版权所有@惠州塑伯新材料有限公司The above data for the theory of the measurement data of our company, for your reference only. Copyright @ Huizhou SPP New Material Co., Ltd.   



      如需了解更多产品信息,请联系我们:

      销售专员:

      廖流爱:13922538943(微信/手机同号)

      李小姐:13826903196(微信/手机同号)

      李明霞:13829234372(微信/手机同号)

      技术支持:

      廖慈华:13602342196(微信/手机同号)




      0
      * 表示必填采购:85S
      * 联系人: 请填写您的真实姓名
      公司名称: 请填写您的公司名称
      联系电话:
      * 手机号码: 请填写您的联系电话
      *QQ:
      联系地址:
      * 采购意向描述:
      请填写采购的产品数量和产品描述,方便我们进行统一备货。
      验证码: 验证码
      我要评论:  
      内 容:
      (内容最多500个汉字,1000个字符)
      验证码: 看不清?!