      倍韧®/BESTPERNE® ES85E-02

      热塑性弹性体Thermoplastic Elastomer

      产品说明Product description


      ·ES85E-02是一款SEBS透明材料,具有优异耐候性和特别舒适的手感。可快速成型。

      ·ES85E-02is a kind of transparent polymer material based on SEBS which has excellent weather resistance and special comfortable touch.Also it can be taken shape rapidly.


      关键特性Key characteristic


      1.表面微亮A little bright on the surface.

      2.成型快,不粘模具Rapid molding,non-stick mold.

      3.耐黄变,耐候性能好Excellent yellowing resistance and weather resistance.

      4.可以包胶PP  It can be spliced with PP.


      功能Function


      产品应用

      Main application

      饭盒盖包胶Rubber coating of lunch-box cover


      玩具产品Toy products

      电子器件粘胶配件Electronic plastic accessories


      加工方法Processing method

      注塑成型Injection molding


      环保认证

      Environmental certification

      ROHS

      REACH

      EN71-3


      PAHS

      ASTM-F963

      Phthalate


      颜色Color

      透明 Translucent


      气味Smell

      少许树脂味A little resin smell


      外型Appearance

      圆球形小颗粒Cylindrical particle,about 3mm×1.5mm


      储藏期Storage period

      常温下通风干燥,24个月Ventilated dry at normal temperature,about 24 months


      包装方式Packaging method

      25公斤/袋 25kg/bag


      物理性能Physical properties

      结果Result

      单位Unit

      方法Method

      成型条件Molding condition


      比重Specific gravity

      0.9±0.02

      g/cm3

      ASTM D792

      干燥温度Drying temp     70 ℃


      硬度Hardness

      85±5

      shoreA

      ASTM D2240

      干燥时间Drying time      2h


      拉伸强度Tensile strength

      >7

      Mpa

      ASTM D412

      射嘴温度Nozzle temp     220℃


      断裂延伸Elongation at break

      >450

      %

      ASTM D412

      螺筒一段温度Screw 1 temp 210℃


      撕裂强度Tearing strength

      >40

      Kn/m

      ASTM D624

      螺筒二段温度Screw 2 temp 190℃


      熔融指数Melt index

      <3

      g/10min

      ASTM D1238

      螺筒三段温度Screw 3 temp 170℃




      如需了解更多产品信息,请联系我们:

      销售专员:

      廖流爱:13922538943(微信/手机同号)

      李小姐:13826903196(微信/手机同号)

      李明霞:13829234372(微信/手机同号)

      技术支持:

      廖慈华:13602342196(微信/手机同号)




      0
      * 表示必填采购:ES85E-02
      * 联系人: 请填写您的真实姓名
      公司名称: 请填写您的公司名称
      联系电话:
      * 手机号码: 请填写您的联系电话
      *QQ:
      联系地址:
      * 采购意向描述:
      请填写采购的产品数量和产品描述,方便我们进行统一备货。
      验证码: 验证码
      我要评论:  
      内 容:
      (内容最多500个汉字,1000个字符)
      验证码: 看不清?!