倍韧/BESTPERNE® TA5522C-1
热塑性弹性体Thermoplastic Elastomer
产品说明Product description | ||||||||
· TA5522C-1是一款流动性高,成型快,耐磨,耐候性好的高分子材料,能够包ABS ,PC材料。 · TA5522C-1is a kind of high flow,excellent wear resistance and weather resistance polymer material which can be spliced with ABS and PC material.Also it can be taken shape rapidly. | ||||||||
关键特性Key characteristic | ||||||||
1. 表面哑,手感细腻柔软。dumb surface, exquisite and soft feeling touch 2. 粘接强度非常高,可粘接材质:ABS.PC. very high bonding strength, adhesive material: ABS, PC. 3. 成型快、不粘模具。rapid molding,non-stick mold 4. 表面耐刮擦,不易起毛屑。scratch resistance on the surface,not easy to fluff | ||||||||
功能Function | ||||||||
产品应用 Main application | 手机保护Phone protective cover | 电子产品Electronic products | ||||||
仪器外壳Instrument shell | 剪刀手柄Handles of scissors | |||||||
加工方法Processing method | 注塑成型Injection molding | |||||||
环保认证 Environmental certification | ROHS | REACH | EN71-3 | |||||
PAHS | ASTM-F963 | Phthalate | ||||||
颜色Color | 本色Natural | |||||||
气味Smell | 少许树脂味A little resin smell | |||||||
外型Appearance | 圆球形小颗粒Cylindrical particle,about 3mm×1.5mm | |||||||
储藏期Storage period | 常温下通风干燥,24个月Ventilated dry at normal temperature,about 24 months | |||||||
包装方式Packaging method | 25公斤/袋 25kg/bag | |||||||
物理性能Physical properties | 结果Result | 单位Unit | 方法Method | 成型条件Molding condition | ||||
比重Specific gravity | 1.062 | g/cm3 | ASTM D792 | 干燥温度Drying temp 90℃ | ||||
硬度Hardness | 58-60A | shoreA | ASTM D2240 | 干燥时间Drying time 2Hours | ||||
拉伸强度Tensile strength | 6 | Mpa | ASTM D412 | 射嘴温度Nozzle temp 200℃ | ||||
断裂延伸Elongation at break | 524 | % | ASTM D412 | 螺筒一段温度Screw 1 temp 190℃ | ||||
撕裂强度Tearing strength | 29.1 | Kn/m | ASTM D624 | 螺筒二段温度Screw 2 temp 180℃ | ||||
熔融指数Melt index | 4.2/2.16KG 190℃ | g/10min | ASTM D1238 | 螺筒三段温度Screw 3 temp 180℃ | ||||
注意事项Matters need attention | ||||||||
清洗料管 Purge compound | 需使用PP或 PE清洗干净机台螺杆,且把机台射嘴彻底清除干净please make sure you that you have cleaned the machine screw with PP or PE, and put the machine nozzle thoroughly clean | |||||||
着色 Coloring
| 请选择以PE或EVA为基材之色母,切勿使用以PVC为基材者。另外加工时请采用较高的螺杆转速和较高的背压,才能让着色剂达到较好的分散效果Please select color master batch on PE or EVA material with the exception of PVC.Higher screw speed and backpressure and needed for better colorant dispersion | |||||||
回收 Recycling | 二次料(水口料)回收比率建议最多20%。 Consistent regrind usage of up to 20% is permissible | |||||||
以上数据为我公司测量之理论数据仅供参考,版权所有@东莞市塑伯橡塑胶有限公司
The above data for the theory of the measurement data of our company, for your reference only. Copyright @ SPP Plastics& Rubber co., LTD
如需了解更多产品信息,请联系我们:
销售专员:
廖流爱:13922538943(微信/手机同号)
谢运英:13826903196(微信/手机同号)
李明霞:13829234372(微信/手机同号)
技术支持:
廖慈华:13602342196(微信/手机同号)
| * 联系人: | 请填写您的真实姓名 |
| * 手机号码: | 请填写您的联系电话 |
| *QQ: | |
| * 采购意向描述: | |
| 请填写采购的产品数量和产品描述,方便我们进行统一备货。 | |
| 验证码: |
|
| 我要评论: | |
| 内 容: |
(内容最多500个汉字,1000个字符) |
| 验证码: | 看不清?! |







共有-条评论【我要评论】