倍韧/BESTPERNE® TA80B-10
热塑性弹性体Thermoplastic Elastomer
产品说明Product description | ||||||||
·TA80B-10是一款高性能新型的高分子材料,具有优异的耐磨、耐污耐旧、耐热性能。 ·TA80B-10 is a new kind of high performance polymer material which has excellent wear resistance,stain resistance,old resistance and heat resistance properties. | ||||||||
关键特性Key characteristic | ||||||||
1.表面微亮,手感细腻柔软爽滑A little bright on the surface,exquisite,smooth and soft touch. 2.粘接强度非常高,可粘接材质:ABS、PC 、TPU Very high bonding strength,adhesive materials:ABS、PC、TPU. 3.超耐磨高强度,高回复性,抗变形Excellent wear resistance and deformation resistance,high strength and resilience. 4.成型快、不粘模具Rapid molding,non-stick mold. | ||||||||
功能Function | ||||||||
产品应用 Main application | 智能腕带Smart bracelet | 手机保护套Phone protective cover | ||||||
仪器外壳Instrument shell | 电子器件粘胶配件Electronic plastic accessories | |||||||
加工方法Processing method | 注塑、挤出成型Injection and extrusion molding | |||||||
环保认证 Environmental certification | ROHS | REACH | EN71-3 | |||||
PAHS | ASTM-F963 | Phthalate | ||||||
颜色Color | 本色Natural | |||||||
气味Smell | 少许树脂味A little resin smell | |||||||
外型Appearance | 圆球形小颗粒Cylindrical particle,about 3mm×1.5mm | |||||||
储藏期Storage period | 常温下通风干燥,24个月Ventilated dry at normal temperature,about 24 months | |||||||
包装方式Packaging method | 25公斤/袋 25kg/bag | |||||||
物理性能Physical properties | 结果Result | 单位Unit | 方法Method | 成型条件Molding condition | ||||
比重Specific gravity | 1.22±0.02 | g/cm3 | ASTM D792 | 干燥温度Drying temp 90 ℃ | ||||
硬度Hardness | 80±5 | shoreA | ASTM D2240 | 干燥时间Drying time 2h | ||||
拉伸强度Tensile strength | >12 | Mpa | ASTM D412 | 射嘴温度Nozzle temp 190℃ | ||||
断裂延伸Elongation at break | >450 | % | ASTM D412 | 螺筒一段温度Screw 1 temp 180℃ | ||||
撕裂强度Tearing strength | >60 | Kn/m | ASTM D624 | 螺筒二段温度Screw 2 temp 170℃ | ||||
熔融指数Melt index | >12 | g/10min | ASTM D1238 | 螺筒三段温度Screw 3 temp 170℃ | ||||
注意事项Matters need attention | ||||||||
清洗料管 Purge compound | 需使用PP或 PE清洗干净机台螺杆,且把机台射嘴彻底清除干净Please make sure you that you have cleaned the machine screw with PP or PE, and put the machine nozzle thoroughly clean. | |||||||
着色 Coloring
| 请选择以PE或EVA为基材之色母,切勿使用以PVC为基材者。另外加工时请采用较高的螺杆转速和较高的背压,才能让着色剂达到较好的分散效果Please select color master batch on PE or EVA material with the exception of PVC.Higher screw speed and backpressure are needed for better colorant dispersion. | |||||||
回收 Recycling | 二次料(水口料)回收比率建议最多20%. Consistent regrind usage of up to 20% is permissible. |
以上数据为我公司测量之理论数据仅供参考,版权所有@惠州塑伯新材料有限公司The above data for the theory of the measurement data of our company, for your reference only. Copyright @ Huizhou SPP New Material Co., Ltd.