倍韧/BESTPERNE® TE7200-1
热塑性弹性体Thermoplastic Elastomer
产品说明Product description | |||||||
·TE7200-1是一款高性能材料,具有非常好的弹性,强度,成型性快。 ·TE7200-1 is a kind of high performance material which has very excellent elasticity and strength.Also it can be taken shape rapidly | |||||||
关键特性Key characteristic | |||||||
1. 高强度,高弹性high strength,high elasticity 2. 耐黄变,耐候性,耐油污,耐化学溶剂性优秀.good yellowing resistance,weather resistance,oil resistance,and chemical solvent resistance 3. 成型快、不粘模具。rapid molding,non-stick mold 4. 耐磨性,抗刮伤优excellent wear resistance and scratch resistance | |||||||
功能Function | |||||||
产品应用 Main application | 垫圈Washer | 眼镜框Spectacle frames | |||||
仪器外壳Instrument shell | |||||||
加工方法Processing method | 注塑成型Injection molding | ||||||
环保认证 Environmental certification | ROHS | REACH | EN71-3 | ||||
PAHS | ASTM-F963 | Phthalate | |||||
颜色Color | 本黄色 Raw yellow | ||||||
气味Smell | 少许树脂味A little resin smell | ||||||
外型Appearance | 圆球形小颗粒Cylindrical particle,about 3mm×1.5mm | ||||||
储藏期Storage period | 常温下通风干燥,24个月Ventilated dry at normal temperature,about 24 months | ||||||
包装方式Packaging method | 25公斤/袋 25kg/bag | ||||||
物理性能Physical properties | 结果Result | 单位Unit | 方法Method | 成型条件Molding condition | |||
比重Specific gravity | 1.2±0.02 | g/cm3 | ASTM D792 | 干燥温度Drying temp 95℃ | |||
硬度Hardness | 72±3 | shoreD | ASTM D2240 | 干燥时间Drying time 3Hours | |||
拉伸强度Tensile strength | >30 | Mpa | ASTM D412 | 射嘴温度Nozzle temp 240℃ | |||
断裂延伸Elongation at break | >250 | % | ASTM D412 | 螺筒一段温度Screw 1 temp 230℃ | |||
撕裂强度Tearing strength | >160 | Kn/m | ASTM D624 | 螺筒二段温度Screw 2 temp 220℃ | |||
熔融指数Melt index | <10 | g/10min | ASTM D1238 | 螺筒三段温度Screw 3 temp 200℃ |