产品说明 Product description
是一款高性能高分子材料,具有非常强劲的包胶粘接强度和特别舒适的手感。可快速成型。
is a kind of high performance polymer material which has very high bonding strength and special comfortable touch.Also it can be taken shape rapidly.
关键特性 Key characteristic
1. 表面哑,手感细腻柔软 Dumb surface,exquisite and soft touch.
2. 可粘接材质:ABS.PC Adhesive materials:ABS and PC.
3. 成型快、不粘模具 Rapid molding,non-stick mold.
4. 表面耐刮擦,不易起毛屑 Scratch resistance on the surface,not easy to fluff.
功能 Function
产品应用 Main application | 仪器外壳 Instrument shell | |||||
加工方法 Processing method | 注塑成型 Injection molding | |||||
环保认证 Environmental certification | ROHS | PAHS | EN71-3 | |||
PAHS | ASTM-F96 | Phthalate | ||||
颜色 Color | 黑色 Black | |||||
气味 Smell | 少许树脂味 A little resin smell | |||||
外型 Appearance | 圆球形小颗粒 Cylindrical particle,about 3mm×1. | |||||
储藏期 Storage period | 常温下通风干燥,24 个月 Ventilated dry at normal temperature,about | |||||
包装方式 Packaging method | 25 公斤/袋 25kg/bag | |||||
物理性能 Physical properties | 结果 Result | 单位 Unit | 方法 Method | 成型条件 Molding condition | ||
比重 Specific grav | 1.2±0.02 | g/cm3 | ASTM D792 | 干燥温度 Drying temp | 90℃ | |
硬度 Hardness | 85±5 | shoreA | ASTM D2240 | 干燥时间 Drying time | 2 小时 | |
拉伸强度 Tensile strength | >20 | Mpa | ASTM D412 | 射嘴温度 Nozzle temp | 200 | |
断裂延伸率 Elongation at break | >560 | % | ASTM D412 | 螺筒三段温度 Screw 1 temp | 190 | |
撕裂强度 Tearing strengt | >90 | Kn/m | ASTM D624 | 螺筒三段温度 Screw 2 temp | 180 | |
熔融指数 Melt indexgravity | >20 | g/10min | ASTM D1238 | 螺筒三段温度 Screw 3 temp | 170 | |
如需了解更多产品信息,请联系我们:
销售专员:
廖流爱:13922538943(微信/手机同号)
李小姐:13826903196(微信/手机同号)
李明霞:13829234372(微信/手机同号)
技术支持:
廖慈华:13602342196(微信/手机同号)
| * 联系人: | 请填写您的真实姓名 |
| * 手机号码: | 请填写您的联系电话 |
| *QQ: | |
| * 采购意向描述: | |
| 请填写采购的产品数量和产品描述,方便我们进行统一备货。 | |
| 验证码: |
|
相关资讯
| 我要评论: | |
| 内 容: |
(内容最多500个汉字,1000个字符) |
| 验证码: | 看不清?! |










共有-条评论【我要评论】