      倍韧/BESTPERNE® ZF45B

      热塑性弹性体Thermoplastic Elastomer

      产品说明Product description

      ZF45B是一款减震高分子材料,耐候性,耐油,耐化学性能优。减震率可达15%,可注塑成型。

      ZF45B is a shock-absorbing polymer materials, durability, oil resistance, high chemical resistance. Shock absorption rate of up to 15% can be injection molded.

      关键特性Key characteristic

      1.表面微亮,手感细腻柔软爽滑.              a little bright on the surface,exquisite,smooth and soft touch feeling.

      2.超耐磨高强度,高回复性,抗变形excellent wear resistance and deformation resistance,high strength and resilience.

      3.成型快、不粘模具.rapid molding,non-stick mold. 

      4.阻尼效果优异.    Damping effect is good.

      功能Function

      产品应用

      Main application

      手机保护套Phone protective cover

      仪器外壳Instrument shell

      电子器件粘胶配件Electronic plastic accessories

      加工方法Processing method

      注塑、挤出成型Injection and extrusion molding

      环保认证

      Environmental certification

      ROHS

      REACH

      EN71-3

      PAHS

      ASTM-F963

      Phthalate

      颜色Color

      本色Natural

      气味Smell

      少许树脂味A little resin smell

      外型Appearance

      圆球形小颗粒Cylindrical particle,about 3mm×1.5mm

      储藏期Storage period

      常温下通风干燥,24个月Ventilated dry at normal temperature,about 24 months

      包装方式Packaging method

      25公斤/袋 25kg/bag

      物理性能Physical properties

      结果Result

      单位Unit

      方法Method

      成型条件Molding condition

      比重Specific gravity

      1.±0.02

      g/cm3

      ASTM D792

      干燥温度Drying temp     60 ℃

      硬度Hardness

      46±5

      shoreA

      ASTM D2240

      干燥时间Drying time      3h

      拉伸强度Tensile strength

      >3

      Mpa

      ASTM D412

      射嘴温度Nozzle temp     200℃

      断裂延伸Elongation at break

      >400

      %

      ASTM D412

      螺筒一段温度Screw 1 temp 190℃

      撕裂强度Tearing strength

      >12

      Kn/m

      ASTM D624

      螺筒二段温度Screw 2 temp 180℃

      熔融指数Melt index

      >3

      g/10min

      ASTM D1238

      螺筒三段温度Screw 3 temp 170℃



      如需了解更多产品信息,请联系我们:

      销售专员:

      廖流爱:13922538943(微信/手机同号)

      李小姐:13826903196(微信/手机同号)

      李明霞:13829234372(微信/手机同号)

      技术支持:

      廖慈华:13602342196(微信/手机同号)




      0
      * 表示必填采购:ZF45B
      * 联系人: 请填写您的真实姓名
      公司名称: 请填写您的公司名称
      联系电话:
      * 手机号码: 请填写您的联系电话
      *QQ:
      联系地址:
      * 采购意向描述:
      请填写采购的产品数量和产品描述,方便我们进行统一备货。
      验证码: 验证码
      我要评论:  
      内 容:
      (内容最多500个汉字,1000个字符)
      验证码: 看不清?!