倍韧/BESTPERNE? EN45A-DF 热塑性弹性体Thermoplastic Elastomer 产品说明Product description EN45A-DF是一款以SEBS为主基材的热
倍韧/BESTPERNE® EN45A-HL
热塑性弹性体Thermoplastic Elastomer
产品说明Product description | |||||||
·EN45A-HL是一款以SEBS为主基材的高性能弹性体,易加工,耐黄变,耐化学溶剂性能非常出色。 ·EN45A-HL is a kind of high performance thermoplastic elastomer based on SEBS as main material.Aslo it has excellent yellowing resistance and chemical solvent resistance properties.It is easy processing. | |||||||
关键特性Key characteristic | |||||||
1.表面哑,手感细腻柔软。Dumb surface, exquisite and soft touch 2.可粘接PP,强度非常高。Very high bonding strength, adhesive material:PP 3.成型快、不粘模具。Rapid molding,non-stick mold | |||||||
功能Function | |||||||
产品应用 Main application | 1 汽车用品 Automotive products | 3手把Handlebar | |||||
2 运动器材Sports equipment | 4玩具产品Toy products | ||||||
加工方法Processing method | 注塑成型Injection molding | ||||||
环保认证 Environmental certification | ROHS | REACH | EN71-3 | ||||
PAHS | ASTM-F963 | Phthalate | |||||
颜色Color | 本色 Natural | ||||||
气味Smell | 少许树脂味A little resin smell | ||||||
外型Appearance | 圆球形小颗粒Cylindrical particle,about 3mm×1.5mm | ||||||
储藏期Storage period | 常温下通风干燥,24个月Ventilated dry at normal temperature,about 24 months | ||||||
包装方式Packaging method | 25公斤/袋 25kg/bag | ||||||
物理性能Physical properties | 结果Result | 单位Unit | 方法Method | 成型条件Molding condition | |||
比重Specific gravity | 1.03±0.02 | g/cm3 | ASTM D792 | 干燥温度Drying temp 70℃ | |||
硬度Hardness | 45±5 | shoreA | ASTM D2240 | 干燥时间Drying time 2Hours | |||
拉伸强度Tensile strength | >2 | Mpa | ASTM D412 | 射嘴温度Nozzle temp 190℃ | |||
断裂延伸Elongation at break | >400 | % | ASTM D412 | 螺筒一段温度Screw 1 temp 190℃ | |||
撕裂强度Tearing strength | >14 | Kn/m | ASTM D624 | 螺筒二段温度Screw 2 temp 180℃ | |||
熔融指数Melt index | >1 | g/10min | ASTM D1238 | 螺筒三段温度Screw 3 temp 180℃ |