      产品说明Product description


      ES65A-MT是一款经济型半透明材料,具有优异的耐刮擦效果。

      ES65A-MT is a kind of economical and translucent material which has excellent scratch resistance property.


      关键特性Key characteristic


      1.表面哑,手感细腻柔软Dumb surface, exquisite and soft touch.

      2.粘接强度非常高,可粘接材质:PP,PE.  Very high bonding strength,adhesive materials:PP and PE.

      3.成型快、不粘模具Rapid molding and non-stick mold.

      4.表面耐刮擦,不易起毛屑Scratch resistance on the surface,not easy to fluff.


      功能Function


      产品应用

      Main application

      饭盒盖包胶Rubber coating of lunch-box cover


      玩具产品Toy products

      电子器件粘胶配件Electronic plastic accessories


      加工方法Processing method

      注塑成型Injection molding


      环保认证

      Environmental certification

      ROHS

      REACH

      EN71-3


      PAHS

      ASTM-F963

      Phthalate


      颜色Color

      半透明 Translucent


      气味Smell

      少许树脂味A little resin smell


      外型Appearance

      圆球形小颗粒Cylindrical particle,about 3mm×1.5mm


      储藏期Storage period

      常温下通风干燥,24个月Ventilated dry at normal temperature,about 24 months


      包装方式Packaging method

      25公斤/袋 25kg/bag


      物理性能Physical properties

      结果Result

      单位Unit

      方法Method

      成型条件Molding condition


      比重Specific gravity

      0.89±0.02

      g/cm3

      ASTM D792

      干燥温度Drying temp     70 ℃


      硬度Hardness

      65±5

      shoreA

      ASTM D2240

      干燥时间Drying time      2h


      拉伸强度Tensile strength

      >4

      Mpa

      ASTM D412

      射嘴温度Nozzle temp     200℃


      断裂延伸Elongation at break

      >450

      %

      ASTM D412

      螺筒一段温度Screw 1 temp 190℃


      撕裂强度Tearing strength

      >18

      Kn/m

      ASTM D624

      螺筒二段温度Screw 2 temp 180℃


      熔融指数Melt index

      >6

      g/10min

      ASTM D1238

      螺筒三段温度Screw 3 temp 170℃


      注意事项Matters need attention


      清洗料管

      Purge compound

      需使用PP或 PE清洗干净机台螺杆,且把机台射嘴彻底清除干净Please make sure you that you have cleaned the machine screw with PP or PE, and put the machine nozzle thoroughly clean.


      着色

      Coloring

       

       

      请选择以PE或EVA为基材之色母,切勿使用以PVC为基材者。另外加工时请采用较高的螺杆转速和较高的背压,才能让着色剂达到较好的分散效果Please select color master batch on PE or EVA material with the exception of PVC.Higher screw speed and backpressure are needed for better colorant dispersion.


      回收

      Recycling

      二次料(水口料)回收比率建议最多20%.

      Consistent regrind usage of up to 20% is permissible.




      如需了解更多产品信息,请联系我们:

      销售专员:

      廖流爱:13922538943(微信/手机同号)

      李小姐:13826903196(微信/手机同号)

      李明霞:13829234372(微信/手机同号)

      技术支持:

      廖慈华:13602342196(微信/手机同号)




      0
      * 表示必填采购:ES65A-MT
      * 联系人: 请填写您的真实姓名
      公司名称: 请填写您的公司名称
      联系电话:
      * 手机号码: 请填写您的联系电话
      *QQ:
      联系地址:
      * 采购意向描述:
      请填写采购的产品数量和产品描述,方便我们进行统一备货。
      验证码: 验证码
      我要评论:  
      内 容:
      (内容最多500个汉字,1000个字符)
      验证码: 看不清?!