      倍韧/BESTPERNE®  TAB75B-17

      热塑性弹性体Thermoplastic Elastomer

      产品说明Product description

      ·TAB75B-17是一款高性能新型的高分子材料,具有优异的耐磨、耐污耐旧、耐热性能。

      ·TAB75B-17 is a new kind of high performance polymer material which has excellent wear resistance,stain resistance,old resistance and heat resistance properties.

      关键特性Key characteristic

      1.表面微亮,手感细腻柔软爽滑A little bright on the surface,exquisite,smooth and soft touch.

      2.粘接强度非常高,可粘接材质:ABS、PC 、TPU  Very high bonding strength,adhesive materials:ABS、PC、TPU.

      3.超耐磨高强度,高回复性,抗变形Excellent wear resistance and deformation resistance,high strength and resilience.

      4.成型快、不粘模具Rapid molding,non-stick mold.

      功能Function

      产品应用

      Main application

      智能腕带Smart bracelet

      手机保护套Phone protective cover

      仪器外壳Instrument shell

      电子器件粘胶配件Electronic plastic accessories

      加工方法Processing method

      注塑、挤出成型Injection and extrusion molding

      环保认证

      Environmental certification

      ROHS

      REACH

      EN71-3

      PAHS

      ASTM-F963

      Phthalate

      颜色Color

      黑色 Black

      气味Smell

      少许树脂味A little resin smell

      外型Appearance

      圆球形小颗粒Cylindrical particle,about 3mm×1.5mm

      储藏期Storage period

      常温下通风干燥,24个月Ventilated dry at normal temperature,about 24 months

      包装方式Packaging method

      25公斤/袋 25kg/bag

      物理性能Physical properties

      结果Result

      单位Unit

      方法Method

      成型条件Molding condition

      比重Specific gravity

      1.14±0.02

      g/cm3

      ASTM D792

      干燥温度Drying temp     90 ℃

      硬度Hardness

      75±5

      shoreA

      ASTM D2240

      干燥时间Drying time      2h

      拉伸强度Tensile strength

      >6

      Mpa

      ASTM D412

      射嘴温度Nozzle temp     190℃

      断裂延伸Elongation at break

      >450

      %

      ASTM D412

      螺筒一段温度Screw 1 temp 180℃

      撕裂强度Tearing strength

      >38

      Kn/m

      ASTM D624

      螺筒二段温度Screw 2 temp 170℃

      熔融指数Melt index

      >3

      g/10min

      ASTM D1238

      螺筒三段温度Screw 3 temp 170℃



      如需了解更多产品信息,请联系我们:

      销售专员:

      廖流爱:13922538943(微信/手机同号)

      李小姐:13826903196(微信/手机同号)

      李明霞:13829234372(微信/手机同号)

      技术支持:

      廖慈华:13602342196(微信/手机同号)




      0
      * 表示必填采购:TAB75B-17 tpu材料供应商
      * 联系人: 请填写您的真实姓名
      公司名称: 请填写您的公司名称
      联系电话:
      * 手机号码: 请填写您的联系电话
      *QQ:
      联系地址:
      * 采购意向描述:
      请填写采购的产品数量和产品描述,方便我们进行统一备货。
      验证码: 验证码
      我要评论:  
      内 容:
      (内容最多500个汉字,1000个字符)
      验证码: 看不清?!